I think this is the best place to post this. Let me know if this should go into another forum. I was asked if there was a standard that stated material up to a certain thickness is call "sheet" and anything above that thickness is called "plate". I can not recall if there is a standard for this or not. Is this a company thing?

Scorch

Don't worry about people stealing your ideas. If your ideas are any good, you'll have to ram them down people's throats.
--Howard Aiken, IBM engineer

 
Replies continue below

Recommended for you

I think it is a company thing. In college, I heard it said that Caterpillar considered anything up to 3" sheet, while Boeing considered anything over 1/8" plate.

Your thicknesses may vary.


"Wildfires are dangerous, hard to control, and economically catastrophic."
"Fixed in the next release" should replace "Product First" as the PTC slogan.

Ben Loosli
CAD/CAM System Analyst
Ingersoll-Rand
 
below 3/16: sheet
3/16 and above: plate
Any mtl spec I look at shows these numbers.

Chris
Sr. Mechanical Designer, CAD
SolidWorks 05 SP1.1 / PDMWorks 05
ctopher's home site
 
There are many ASTM standards for steel sheet and plate. ASTM A 635 reflects sheet up to one inch.


John
 
The ASM glossary of terms reports the following:

plate
A flat-rolled metal product of some minimum thickness and width arbitrarily dependent on the type of metal. Plate thicknesses commonly range from 6 to 300 mm (0.25 to 12 in.); widths from 200 to 2000 mm (8 to 80 in.).

sheet
A flat-rolled metal product of some maximum thickness and minimum width arbitrarily dependent on the type of metal. It has a width-to-thickness ratio greater than about 50. Generally, such flat products under 6.5 mm (1/4 in.) thick are called sheets, and those 6.5 mm (1/4 in.) thick and over are called plates.



 