Sep 10, 2017 #1 johnlabuu Petroleum Joined Sep 10, 2017 Messages 8 Location MY Dear All Engineer's, What electrode or filler rod to weld pipe material AISI 4130? We're in the middle on prepared the new PQR & WPS for material 4130. Please someone advise me. Thanks
Dear All Engineer's, What electrode or filler rod to weld pipe material AISI 4130? We're in the middle on prepared the new PQR & WPS for material 4130. Please someone advise me. Thanks
Sep 11, 2017 #2 gtaw Structural Joined Feb 10, 2006 Messages 1,985 Location US What welding process do you plan to use? ESAB makes a filler metal for 4130. Best regards - Al Upvote 0 Downvote
Sep 12, 2017 Thread starter #3 johnlabuu Petroleum Joined Sep 10, 2017 Messages 8 Location MY We plan to using GTAW process. Upvote 0 Downvote
Sep 12, 2017 #4 Mr168 Materials Joined Aug 5, 2008 Messages 731 Location US Postweld heat treatment or as-welded condition? Upvote 0 Downvote
Sep 13, 2017 Thread starter #5 johnlabuu Petroleum Joined Sep 10, 2017 Messages 8 Location MY Im not familiar with this material requirement. Im welding pipe with diameter 6" with thickness 21mm. Ambient temperature. Please advise sir. Upvote 0 Downvote
Im not familiar with this material requirement. Im welding pipe with diameter 6" with thickness 21mm. Ambient temperature. Please advise sir.