Dear All Engineer's,
What electrode or filler rod to weld pipe material AISI 4130?
We're in the middle on prepared the new PQR & WPS for material 4130.
Please someone advise me.
Thanks
 
What welding process do you plan to use?

ESAB makes a filler metal for 4130.

Best regards - Al
 
Postweld heat treatment or as-welded condition?
 
Im not familiar with this material requirement.
Im welding pipe with diameter 6" with thickness 21mm.
Ambient temperature.
Please advise sir.
 