Hi,

I am looking at a design example on shear lug weld design in AISC DG 1. For the shear lug weld check, the DG does not use directionality factor for designing the welds. Is there a reason for that? The forces are pretty much perpendicular to the weld. why cant directionality factor of 1.5 be used for the weld design?

Thanks
 
Replies continue below

Recommended for you

Weld directionality is a relatively recent addition to the AISC spec I believe, came into CSA S16 first and then went in AISC when I was still an EIT maybe ~10 years ago iirc? The first printing of 2nd edition DG1 (is there a more recent edition?) was 2006, and since this isn't an error I doubt they'd go back and revise the check. Just my guess though, someone should confirm there isn't another reason or I'm not out to lunch on the dates.
 