We have some custom stainless steel tools with hole saw type geometry where the cutting 'tips' are not of a standard geometry--it has a scalloped leading edge which creates two sharp 'peaks' at the innermost and outermost edges:

View attachment 8604

These items are intended for limited re-use, but we would like to be able to determine (in-between uses) when they are no longer "sharp enough" without requiring complicated/time-consuming/expensive metrology such as was necessary when they were first manufactured. Presently there is a visual inspection (minor magnification only) that should weed out ones that are obviously damaged (e.g. fractured/bent edges) but can not reliably determine when it is simply 'dull'. Therefore, if I can find examples of various levels of dullness (determined subjectively), can we develop a way to 'measure' them somehow in a fashion that can be adapted for a relatively non-skilled technician to evaluate?

Curious to know what may already be out there to evaluate something like this. A thought thus far would be to somehow use pressure sensitive film (or similar) under a (non-destructive) controlled axial load to evaluate the contact patterns created... but my exposure (pun intended) to using said film is mostly tales of how knee replacement devices were developed/evaluated and nothing practical.

Any obvious ideas?
 
I don't know if this guy has a video to cover your problem, but I can't think of anyone better - https://www.youtube.com/@OUTDOORS55/videos

He has made a full scientific analysis of how knife blades are actually sharp and how thing get dull and has microscopic evidence to support what he shows at the macroscopic level.
 
Can't see your attachment, so unclear what your edge actually looks like.

Nevertheless, the Youtuber that Greg cited uses a sharpness tester that uses the amount of force required to cut through a calibrated wire on the tester to determine absolute sharpness. Note, however, the tester is designed for testing knife edges, so other types of edges likely will produce drastically different results.

https://www.sharpeningsupplies.com/...JafIrDyzGw_9lM6c54oJcbzqkdkmZDLbho-MKBDhpbywA
 
Can't see your attachment, so unclear what your edge actually looks like.

Well, that's a tease--it shows up in the post preview before submitting. I tried it a little different way:

Screenshot 2025-04-23 143205.png
 
That's a challenging geometry for the typical sharpness tester.

Which direction is rotation? I think it's CCW in your image, based on your OP description. Aside from a modification of the commercial sharpness tester or a high magnification visual inspection, the only other thing I can think of is some sort of load measurement, i.e., how hard does the machine have to work to make progress in the cutting, like motor current.
 
You might be able to use a Best tester with some special fixturing.
but I am more with IR on this.
Measuring load (torque) may be your best option.
We had CNC lathes that had a carbon steel backing plate that was replaceable.
After every few pieces there was a cut taken from the edge of the backing plate.
We measured the load for these cuts and used this to predict tool changes.
 
Which direction is rotation? I think it's CCW in your image, based on your OP description.
CCW as illustrated in the picture, yes.

Torque/load to cut may be an option if we can identify a suitable medium that doesn't in itself cause undue abrasion. Will have to kick that around.

One thing I intentionally didn't mention since it's related but presently out-of-scope, is that the alloy that was chosen by the original designers is 17-4 in H900 which is not doing any favors for edge retention... I'm not really sure why 17-4 was selected other than the availability and familiarity of the material at the current manufacturer (there are some questionable tolerances as well, which may make using non-PH grades a little more challenging). Maybe that material selection can eventually be revisited and reduce the opportunity for 'dulling' -- although resulting losses in ductility may cause unwanted changes in failure mode during use [yinyang].
 
Any surface treatments?
17-4 will only get you in the low to mid 40's HRC.
With tool steels you are dealing with mid-50's into the low 60's.
What are you cutting?
 
No surface treatments. Cutting articular cartilage, cortical and cancellous bone. I'm still not convinced how often we are seeing dullness that was induced by direct cutting of the tissues, but that doesn't completely obviate the need to assess the sharpness if only to say that we do/can as there are opportunities for contact with other materials (intentional or unintentional) during use or during cleaning/transit/etc.
 
Perhaps you can find a plastic that has toughness/hardness similar to cartilage to use for an assessment.
 