I'll post this in a couple forums.
We're looking at pump shafts, under 6" bar size. Other than the 10 points difference in Carbon content (per ASTM A29), I can't find an appreciable difference between 4140 and 4150 until you get around 8" bar size where tensile differs a little.
Assuming non-resulfurized, is there any reason - such as machining - that makes one better?
Thanks! Keep the wheels on the ground
Bob
showshine@aol.com
We're looking at pump shafts, under 6" bar size. Other than the 10 points difference in Carbon content (per ASTM A29), I can't find an appreciable difference between 4140 and 4150 until you get around 8" bar size where tensile differs a little.
Assuming non-resulfurized, is there any reason - such as machining - that makes one better?
Thanks! Keep the wheels on the ground