Hi, currently we have a problem at the gas plant i work for.
we have a dehydration system it consists of the following:
a horizontal separator vessel to separat the free water up to 10 microns in the feed gas, after which the feed gas enters a filter coellescer to separate water particles up to 1 micron.
after that feed gas enters molecular sieve adsorption system to be dyhedrated.
what we noticed is that the valves at the bottom of the separator and the filter don't open which means that we don't separate any liquid from the feed gas so we invistigated it and realised that the separator is undersized, we installed a van pack and then a retrofit ( inlet deflector & Demister) and in both time the valves opened wide opens for a couple of days and then closed again.
we now realize that everytime the vessel is opened it has a high performance and then after couple of days something happens which decreases the performance, we are running a root case analysys and currently lookinf for any possible causes so could anybody help.
if any further information is required please feel free to ask, thanks in advance.
we have a dehydration system it consists of the following:
a horizontal separator vessel to separat the free water up to 10 microns in the feed gas, after which the feed gas enters a filter coellescer to separate water particles up to 1 micron.
after that feed gas enters molecular sieve adsorption system to be dyhedrated.
what we noticed is that the valves at the bottom of the separator and the filter don't open which means that we don't separate any liquid from the feed gas so we invistigated it and realised that the separator is undersized, we installed a van pack and then a retrofit ( inlet deflector & Demister) and in both time the valves opened wide opens for a couple of days and then closed again.
we now realize that everytime the vessel is opened it has a high performance and then after couple of days something happens which decreases the performance, we are running a root case analysys and currently lookinf for any possible causes so could anybody help.
if any further information is required please feel free to ask, thanks in advance.