Hi. I'm struggling to select the right mech properties for a S235 or S275 steel. I´m not sure if JR is Ok or I should go to a J0 or J2.
location: Uzbekistan
I got the following outdoor temperature (°C)
Monthly average: 1.5 (jan);3.0(Feb);8.2 (Mar)...13.9(oct); 8.1(nov); 4.1(Dec)
Average annual: 14.8
Absolute min: -20.5
Average max of the coldest month: -2.4
As you can see from monthly/annual average JR looks suitable, but the average of coldest month suggests me to select J2.
J0: 3.5% increase of material cost relative to JR
J2: 4% increase of material cost relative to JR