Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

SELECTING SEAT MATERIAL FOR BUTTERFLY VALVE

Status
Not open for further replies.

wsuengineer

Mechanical
Joined
Oct 2, 2006
Messages
11
Location
US
I AM IN SEARCH OF A COMPATIBILITY CHART FOR PROPYLENE GLYCOL (DOWFROST HD) WHEN SELECTING SEAT MATERIALS FOR BUTTERFLY VALVES. SPECIFICALLY: EPDM, NBR, PTFE, SINCE THESE ARE THE MOST COMMON AND LEAST EXPENSIVE.

THANKS.


 
JIMCASEY, I was unable to locate the durco technical document DVATB0004. Will you help me find it.

Thanks,
 
wsuengineer:

go to
There's a box on the left hand side which says "Literature."
Scroll down until you get to document.



Patricia Lougheed

Please see FAQ731-376 for tips on how to make the best use of the Eng-Tips Forums.

Want to post an image? Look at the FAQ's in forum559
 
PROBLEM: CONFLICTING MATERIAL COMPATABILITY FOR 60ºF-130º AT 100PSIG PROPYLENE GLYCOL (DOWFROST HD.

SOURCE
AST, MECHANICAL SEAL MATERIAL SELECTION GUIDE
NBR:NO
EPDM:NO
VITON:YES

SOURCE
CHEMICAL RESISTANCE GUIDE FOR ELASTOMERS II
NBR:YES UP TO 250ºF
EPDM:YES UP TO 70ºF
VITON:YES UP TO 140ºF

SOURCE
NIBCO CHEMICAL RESISTANCE GUIDE FOR VALVES AND FITTINGS
NBR:YES UP TO 180ºF
EPDM:YES UP TO 70ºF
VITON:YES UP TO 140ºF

SOURCE
CAT PUMPS, CHEMICAL COMPATABILITY GUIDE
NBR:YES
EPDM:N/A
VITON:YES

SOURCE
MCNALLY INSTITUE, O-RING SELECTION
NBR:YES
EPDM:N/A
VITON: N/A

SOURCE
GEORG FISCHER, CHEMICAL RESISTANCE
NBR:YES UP TO 68ºF
EPDM:YES UP TO 104ºF
VITON: YES UP TO 104ºF

SOURCE
COLE-PARMER, CHEMICAL COMPATABILITY
NBR:YES
EPDM:YES
VITON: YES

SOURCE
BRAY CONTROLS, MATERIAL SELECTION GUIDE
NBR:YES
EPDM:YES, PREFERED
VITON: YES

SOURCE
PARKER SEALS, FLUID COMPATIBILITY GUIDE
NBR:NO
EPDM:YES
VITON: NO

SOURCE
VIKING, TECHINICAL DATA, FIREFIGHTER ELIMINATOR C
NBR:YES
EPDM:YES
VITON: YES


WHICH WOULD YOU SELECT. I WOULD RATHER GO WITH EPDM OR NBR INSTEAD OF VITON DUE TO THE COST.
 