PROBLEM: CONFLICTING MATERIAL COMPATABILITY FOR 60ºF-130º AT 100PSIG PROPYLENE GLYCOL (DOWFROST HD.
SOURCE
AST, MECHANICAL SEAL MATERIAL SELECTION GUIDE
NBR:NO
EPDM:NO
VITON:YES
SOURCE
CHEMICAL RESISTANCE GUIDE FOR ELASTOMERS II
NBR:YES UP TO 250ºF
EPDM:YES UP TO 70ºF
VITON:YES UP TO 140ºF
SOURCE
NIBCO CHEMICAL RESISTANCE GUIDE FOR VALVES AND FITTINGS
NBR:YES UP TO 180ºF
EPDM:YES UP TO 70ºF
VITON:YES UP TO 140ºF
SOURCE
CAT PUMPS, CHEMICAL COMPATABILITY GUIDE
NBR:YES
EPDM:N/A
VITON:YES
SOURCE
MCNALLY INSTITUE, O-RING SELECTION
NBR:YES
EPDM:N/A
VITON: N/A
SOURCE
GEORG FISCHER, CHEMICAL RESISTANCE
NBR:YES UP TO 68ºF
EPDM:YES UP TO 104ºF
VITON: YES UP TO 104ºF
SOURCE
COLE-PARMER, CHEMICAL COMPATABILITY
NBR:YES
EPDM:YES
VITON: YES
SOURCE
BRAY CONTROLS, MATERIAL SELECTION GUIDE
NBR:YES
EPDM:YES, PREFERED
VITON: YES
SOURCE
PARKER SEALS, FLUID COMPATIBILITY GUIDE
NBR:NO
EPDM:YES
VITON: NO
SOURCE
VIKING, TECHINICAL DATA, FIREFIGHTER ELIMINATOR C
NBR:YES
EPDM:YES
VITON: YES
WHICH WOULD YOU SELECT. I WOULD RATHER GO WITH EPDM OR NBR INSTEAD OF VITON DUE TO THE COST.