Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Section IX - welder qualifications MIN allowable to wall thickness

Status
Not open for further replies.

Eireann

Petroleum
Jul 10, 2014
1
I have been reviewing some welder qualifications for a small bore 2" piping job sch 80 , the wall thickness is .218 .. The welder "tickets" shows qualification of .250 - max from 1" OD and up . My question is does he qualify to weld on this material as it is thinner than the material he qualified on ? I have heard conflicting reports that there is no minimum deposit thickness qualifications . I am struggleing to find a clear answer in ASME IX. any help or clarity would be appreciated.
 
Replies continue below

Recommended for you

There is no minimum thickness for welder performance qualification, as described in QW-452. In other words the welder is qualified to weld up to the thickness qualified.
 
ASME IX does not tell about minimum qualified thickness for welder/ welding operator as Welder is qualified upto .25 so he can weld .218 thickness. besides this you can not overlook diameter restrictions of ASME IX for welder/ welding operators so check qualified Diameter ranges and compare it with job
 
Qualification on the 0.218" wall pipe permits the welder to weld all thicknesses up to 0.436" wall, assuming the welding process was not the short-circuiting transfer mode of the GMAW process, in which case, he would be qualified to 1.1 x 0.218".
 