Hello All,
I rarely work under Section 9, so please have patience.
An upcoming job requires full penetration butt welds on 4-inch NPS Sched 10 pipe for a hot water application and the designers have applied B31.3 “normal” service criteria.
In my file I have a procedure for GTAW on P-51 which was qualified on 3/8” plate, open root wherein backing and trailing gases were used. The material used during PQR was plate certified to SB-265 Grade 2 which puts it in Group P-51. No impact tests were done on this PQR.
Since the production job is calling for ASTM B862 Grade 2, also in group P-51, I feel my qualified plate procedure is applicable.
However, QW-256 imposes QW-403.6 as a supplementary essential and this states that the minimum thickness qualified is equal to the thickness of the test coupon thickness, which was 3/8”. So does this QW-403.6 render me ineligible to weld .120”thick Sched 10 pipe?
It seems that supplementary essentials are only applied when notch toughness is a requirement – and I don’t see that B31.3 has levied a notch toughness requirement on this application.
All advice and comments appreciated. Tthankyou.
I rarely work under Section 9, so please have patience.
An upcoming job requires full penetration butt welds on 4-inch NPS Sched 10 pipe for a hot water application and the designers have applied B31.3 “normal” service criteria.
In my file I have a procedure for GTAW on P-51 which was qualified on 3/8” plate, open root wherein backing and trailing gases were used. The material used during PQR was plate certified to SB-265 Grade 2 which puts it in Group P-51. No impact tests were done on this PQR.
Since the production job is calling for ASTM B862 Grade 2, also in group P-51, I feel my qualified plate procedure is applicable.
However, QW-256 imposes QW-403.6 as a supplementary essential and this states that the minimum thickness qualified is equal to the thickness of the test coupon thickness, which was 3/8”. So does this QW-403.6 render me ineligible to weld .120”thick Sched 10 pipe?
It seems that supplementary essentials are only applied when notch toughness is a requirement – and I don’t see that B31.3 has levied a notch toughness requirement on this application.
All advice and comments appreciated. Tthankyou.