2
III NH has properties for 2 1/4Cr-1Mo. I would like to know the UNS number of this alloy? Where can I find the UNS for the alloys listed in NH?
Thanks.
 
Replies continue below

Recommended for you

Wrought form UNS K21590,
Castings UNS J21890, J22091 see Section II, Part D
 
Thanks. But Section II D also lists UNS K21390 (bar form) for this nominal composition. So, I am confused.
 