In material specification SECC F20, what does the F20 mean?

This post has also been posted under Mechanical, thanks NickE and SolarMechE for your correspondence
 
Replies continue below

Recommended for you

Are you using a print like the ones I see here at work?

(Faxed, photo-copied 35 times, scribbled on, etc....)

Just seems too much of a coincidence that F20 is what you are reading and F is not a modifier, while E is the standard modifier for electrogalvanized coating weight.
 