Could you provide the density of SECC (Cold rolled, zinc-galvanized steel plate)? I don't have the standard of JIS G 3313.

Thanks!
 
You wouldn't find the mass density in the standard. For low carbon steels like this, a standard figure is 7.87 [·] 103 kg/m3.

Regards,

Cory

Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
Thanks, Cory. Probabaly I need to add 20 g/m2 zinc coating to 7.87x103 kg/m3.

Nava
 
The thickness variation on sheet metal will overwhelm any contribution from the zinc coating.