Hi guys!
I'm trying to find a reference for Seat test pressure and hold time for a check valve we have dissasembled and now reassembled as part of maintenance.
Typically we deliver acc. API 6A.
As far as i can tell API 6A does not mention testing in the context of maintenance?
11.2.4 and Table 32 suggest test pressure to RWP and 3x3min. We were hoping to get away with just one hold period (we have upto 600 check valves to test
)
Thank you!
Regards
Siggi
I'm trying to find a reference for Seat test pressure and hold time for a check valve we have dissasembled and now reassembled as part of maintenance.
Typically we deliver acc. API 6A.
As far as i can tell API 6A does not mention testing in the context of maintenance?
11.2.4 and Table 32 suggest test pressure to RWP and 3x3min. We were hoping to get away with just one hold period (we have upto 600 check valves to test
![[dazed] [dazed] [dazed]](/data/assets/smilies/dazed.gif)
Thank you!
Regards
Siggi