Milkboy
Mechanical
- Mar 13, 2002
- 126
I am seeing an excessive leakage (6ml/hr) when sealing a Water Based Primer Paint. Expected to be 1 to 2 ml/hr with Sic v Sic.
IMO you look to face lapping when you have a constant leakage rate which is high.
However a question has been raised where I have been asked if the paint 'particles' suspended in the water base can
get in between the faces.
The theory being that the particles will tend to the core of the seal/shaft as the heavier water centrifuges outwards.
Any thoughts on this guys and gals ?
-
Milkboy
IMO you look to face lapping when you have a constant leakage rate which is high.
However a question has been raised where I have been asked if the paint 'particles' suspended in the water base can
get in between the faces.
The theory being that the particles will tend to the core of the seal/shaft as the heavier water centrifuges outwards.
Any thoughts on this guys and gals ?
-
Milkboy