Jan 30, 2025 #1 V vhp 16 TSTC Mechanical Joined Jan 30, 2025 Messages 3 In hydraulic (Fluid Power) application seals made with PFAS are used frequently. There are coming restrictions on the use of PFAS. Are there alternatives in sealing technology for hydraulics/
In hydraulic (Fluid Power) application seals made with PFAS are used frequently. There are coming restrictions on the use of PFAS. Are there alternatives in sealing technology for hydraulics/
Feb 26, 2025 #2 bcd Mechanical Joined Sep 27, 2002 Messages 519 Location US Yes there is. Non-PFAS polymers and elastomers, and metal seal options.