Hello!
I have some questions based on the ASTM B571 in the scrib-grid test (paragraph 13) for metal coatings (electrolityc nickel) and plastic as the substrate.
Info to put you in context
- Some of the parts are too small to conduct the test since there are no proper area to perform it.
- Test performed once a month on one piece.
- Found some detached nickel on the tape on last month test.
- Some parts pass the test and others failed, even with minutes of diference in production line.
Questions:
1.- It is possible and appropiate to conduct the test?
2.- If the parts are too small to conduct the test, it is posible to do it in a coupon?
3.- It is necessary to perform the test since the substrate its plastic and not a metal?
4.- Any other test may be applied on plastic?
5.- Detached parts on the tape might have something to do with how the test is perform (strenght, scribs, angle of application,etc.)
6.- Any ideas of what might be changing since the test passed and failed from one WO (work order) to another?
Any other comments are welcome!
Thank you!