Jul 21, 2005 #1 KalleH Structural Joined Sep 16, 2004 Messages 17 Location FR Does anyone have a reference for the relaxation of screw joints in micrometer as function of aspects such as surface roughness and paint type and paint thickness? Thanks!
Does anyone have a reference for the relaxation of screw joints in micrometer as function of aspects such as surface roughness and paint type and paint thickness? Thanks!
Jul 21, 2005 #2 diamondjim Mechanical Joined Jul 30, 2000 Messages 992 Location US Do not use paint on interfaces. Upvote 0 Downvote
Jul 22, 2005 Thread starter #3 KalleH Structural Joined Sep 16, 2004 Messages 17 Location FR That is easy to say if you are not in the heavy vehicle business, where this is standard on chassis, to which brackets are bolted. Upvote 0 Downvote
That is easy to say if you are not in the heavy vehicle business, where this is standard on chassis, to which brackets are bolted.
Jul 23, 2005 #4 Tmoose Mechanical Joined Apr 12, 2003 Messages 5,636 Location US Someone else posted this fine link. http://www.tech.volvo.se/standard/docs/551121.pdf Section 5.3 discusses a factor to be applied to painted joints Upvote 0 Downvote
Someone else posted this fine link. http://www.tech.volvo.se/standard/docs/551121.pdf Section 5.3 discusses a factor to be applied to painted joints
Jul 25, 2005 Thread starter #5 KalleH Structural Joined Sep 16, 2004 Messages 17 Location FR I was probably the one who posted the link to the Volvo standards. However, 5.3 is just about torque/tension relationships. Upvote 0 Downvote
I was probably the one who posted the link to the Volvo standards. However, 5.3 is just about torque/tension relationships.
Jul 25, 2005 #6 CoryPad Materials Joined Apr 15, 2002 Messages 5,192 Location US VDI 2230 has information regarding stress relaxation as a function of surface roughness. VDI 2230 is available from Beuth at: http://www.beuth.de Regards, Cory Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora. Upvote 0 Downvote
VDI 2230 has information regarding stress relaxation as a function of surface roughness. VDI 2230 is available from Beuth at: http://www.beuth.de Regards, Cory Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
Aug 9, 2005 #7 diamondjim Mechanical Joined Jul 30, 2000 Messages 992 Location US We have provided painted structures for heavy equipment and used plugs to prevent painted surfaces under the washers etc. Upvote 0 Downvote
We have provided painted structures for heavy equipment and used plugs to prevent painted surfaces under the washers etc.