Hi everybody;
We are producing reinforcing steel bars. We have some scratch on rebar rib. we saw scratches on 3 or 4 ribs on one 12 meter rebar. Billet does not have any defect like crack. Can you explain reason of this cracks on ribs? Thanks in advance
 
In Europe, the %C for rebar is limited to (somewhere around) .43%, whereas railroad track is pearlitic (.6-.7 %C). Must be an american thing then?
 
Hello

Who still folowing the issure of crack on rebar?
Anyone??
 