hkiremitci

Materials
Apr 4, 2003
8
Hi everybody;
We are producing reinforcing steel bars. We have some scratch on rebar rib. we saw scratches on 3 or 4 ribs on one 12 meter rebar. Billet does not have any defect like crack. Can you explain reason of this cracks on ribs? Thanks in advance
 
Replies continue below

Recommended for you

In Europe, the %C for rebar is limited to (somewhere around) .43%, whereas railroad track is pearlitic (.6-.7 %C). Must be an american thing then?
 