There are a couple of good ferernces published by the Nickel Institute (formerly NiDI). They cover this in detail.
You can download them from the web site.
a lot will depend on the pump size, the duty, the life required from the unit and how much money you have to spend. materials could range from el-cheapo cast iron all the way through to monel.