What temperature will be considered to be safe for Austenitic Stainelss steel for continuous heating application ? If it is heated continuously/intermittently to 300 degrees centigrade, is there any metallurgical deterioration ?
 
Replies continue below

Recommended for you

There will be somme decline in tensile properties. Design codes have taken this into account.
 
There is no metallurgical degradation. Once the material is cooled back to ambient temperature, the tensile properties return to original reported properties.
 
At 300C, even for very long term there will not be any metallurgical damage to any SS grade that I know of.
The strength and modulus will both be slightly lower at temp, but not much at this low of a temp.

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
 
If the temperature is just 300C, why do you need to consider expensive austenitic stainless steels. You can try some of the other alternatives.

_____________________________________
"It's better to die standing than live your whole life on the knees" by Peter Mayle in his book A Good Year
 
300C only ? I have been designing for many units using high carbon content 304H SS and continuously cooking at 730C. No one ever ask how long it will last or fail.
 
Thanks for clarifying. Are the above comments applicable if temperature is 500 degrees centigrade ?
 
Varoon,this is not a Yes or No forum. It provides you guidance and you should make the final call. I think,you should exercise your discretion. Also,next time,please provide more details of your service conditions,existing practice and challenges,to make the discussion more meaningful.

_____________________________________
"It's better to die standing than live your whole life on the knees" by Peter Mayle in his book A Good Year
 
Varoon, you've repeated this question for both 300 deg and 500 deg, for both CS and SStl in two different questions on the forum - but without any supporting details or information in either question.

 