Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations KootK on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

SAE J 429 Grade 8 Bolts for piping applications

Status
Not open for further replies.

Sam35

Mechanical
Sep 14, 2003
19
Are SAE J 429 Grade 8 bolts acceptable for use in a piping system built to B31.3. Does B31.3 recognize Grade 8 bolts?
 
Replies continue below

Recommended for you

No, Grade 8 bolting is not permissable, violation of material and grade.

Rather you need ASTM A193-B7 or B7M studs with ASTM A194-2H or 2HM heavy hex nuts. The "B7M" and "2HM" alternatives conform to the NACE MR-01-75 specification.

The ANSI B31.3 takes into consideration the stress level of bolting and material under various conditions, not only load and temperature. Therefore Charpy Notch Toughness and SCC issues, which directly relate to material considerations, come into play.