What's the difference between SAE-Grade-5 ASTM A449 and ASTM A325?

Both are Medium Carbon, Quenched and Tempered; Proof Load = 85,000 psi; Tensile Strength = 120,000 psi.

Is Grade 5 an acceptable substitution?

Thank you!
 
Replies continue below

Recommended for you

CANPRO... Thank you for your reply.

After speaking with Portland, the major difference between the two is that the A325 has a 1/8" greater heavy hex head which is critical for the tensile application that i was inquiring about.