Can someone point me out what is the material code section 2 part A for the flat washer? I used to know A193 B7,B8,B8M for bolts, A194 2H,8,8M for nuts, but i don't know what is the code for flat washer[ponder].. Thanks for help.
 
wcw1985, there isn't any so far as I know. For hardened flat washers, use ASTM F-436