There is an ongoing discussion in my workplace regarding
SA 516 Gr. 70N vs SA 516 Gr. 70NACT vs SA 516 Gr70 Q&T
Which one is a better heat treatment for SA 516 Gr. 70? The requirement calls for HIC-resistant steel, too.
The group specifications mentioned "minimum normalized" condition for SA 516, and any deviation from this specification is rejected as it "does not meet the specification".
For example, supplying Q&T is deemed not meeting the requirement.
Any thoughts?
SA 516 Gr. 70N vs SA 516 Gr. 70NACT vs SA 516 Gr70 Q&T
Which one is a better heat treatment for SA 516 Gr. 70? The requirement calls for HIC-resistant steel, too.
The group specifications mentioned "minimum normalized" condition for SA 516, and any deviation from this specification is rejected as it "does not meet the specification".
For example, supplying Q&T is deemed not meeting the requirement.
Any thoughts?