Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

SA 234 WPB Pipe caps 1

Status
Not open for further replies.

djmret

Mechanical
Aug 16, 2006
4
What is the MAWP of SA 234 WPB welded pipe caps and where can the information be found?
 
Replies continue below

Recommended for you

djmret,

As far as I know there is no MAWP related to the pipeschedule of a pipecap in the ASME Code. Just make a calculation for an ellipsoidal head.

Good luck
 
I don't know that I've seen anything that actually says what the shape of a pipe cap is.
 
Don't the fitting standards specify the ratings? I was thinking fittings were rated for the MAWP of the pipe of like schedule.

Regards,

Mike
 
The information can be found in ASME B16.11 for forged fittings, socket-welded and threaded.
 
Pipe cap is actually a 2:1 semi-ellipsoidal dished head. Therefore, refer to UG-32 to calculate the MAWP of pipe cap.
 
SA-234 is covered in ASME B16.9 Factory-Made Wrought Buttwelding Fittings.

NozzleTwister
Houston, Texas
 
Hi all,

PEHasan, I'd suggest that you approach your weld cap supplier for some dimensions of the weld caps.UG-32 design for 2:1 semi-ellipsoidal heads require the head shape to be truly ellipsoidal, or if manufactured using two radii then the crown radius must be 0.9D and knuckle 0.17D.Most weld cap suppliers I've encountered manufacture their caps using two radii, that are not necessarily within the 0.9D, 0.17D limits.This would mean that the UG-32 design for 2:1 S/E heads will not be valid for the weld cap.It would need to be designed to Appendix 1.
John
 
ASME B16.9 table I-10 (Dimensions of Caps), General Note (2) indicates that "The shape of these caps shall be ellipsoidal and shall conform to the shape requirements as given in the ASME Boiler and Pressure Vessel Code."

Given that, if a manufacturer tells me that their cap conforms to ASME B16.9, then I can assume that the shape is ellipsoidal, and thus these formulas should apply.

Any thoughts?
 
If used for piping (B31.3) the cap does not need to be calculated. It shall be the same thickness as the calculated pipe wall. So the maximum allowable pressure is depending on the temperature and the selected schedule size.
 