timsch
Mechanical
- Oct 27, 2009
- 193
I have a design using SA 182 Gr. F9 material for a sampling thermowell/quill that will consist of an SA 182 Gr. F9 flange and F9 bar. The bar will have a 1/4" diameter bore and the components will be full-pen welded. The customer has reviewed our weld procedure which has no record of impact testing and has submitted comments stating that the base metal thickness is limited by curve B of Figure 323.2.2A. I have been unable to see that this material is covered by curve B. Table 1A lists a minimum temperature rather than a letter code for a curve for SA 182 Gr. F9.
Am I missing something?