May 12, 2014 #1 radd02 Industrial Joined Apr 30, 2013 Messages 8 Location US A job requirement lists normalized material. I have an MTR that lists this flange as heat treated (normalized). But the mtr copy lists the part as SA-105, not SA-105N. Does the flange itself need the "N" stamp on it for verification?
A job requirement lists normalized material. I have an MTR that lists this flange as heat treated (normalized). But the mtr copy lists the part as SA-105, not SA-105N. Does the flange itself need the "N" stamp on it for verification?
May 12, 2014 #2 JohnGP Mechanical Joined Nov 24, 2003 Messages 475 Location AU SA-105 doesn't require the "N" to be stamped on the flange, unless specified in the order as a supplementary requirement (S2.4). Cheers, John Upvote 0 Downvote
SA-105 doesn't require the "N" to be stamped on the flange, unless specified in the order as a supplementary requirement (S2.4). Cheers, John
May 13, 2014 #3 SnTMan Mechanical Joined Jan 22, 2005 Messages 6,868 Location US Might consult the flange specification, whatever it may be. Regards, Mike Upvote 0 Downvote