A job requirement lists normalized material. I have an MTR that lists this flange as heat treated (normalized). But the mtr copy lists the part as SA-105, not SA-105N. Does the flange itself need the "N" stamp on it for verification?
 
Replies continue below

Recommended for you

SA-105 doesn't require the "N" to be stamped on the flange, unless specified in the order as a supplementary requirement (S2.4).
Cheers,
John
 
Might consult the flange specification, whatever it may be.