Jan 21, 2021 #1 cerbero Industrial Joined Jan 21, 2021 Messages 1 Location CO I NEED to weld sa 105 sa 69 alky, please to inform about electrodes or consumables for process smaw and gtaw.
I NEED to weld sa 105 sa 69 alky, please to inform about electrodes or consumables for process smaw and gtaw.
Jan 22, 2021 #2 weldstan Materials Joined Jun 24, 2011 Messages 2,808 Location US ASTM A-69 has been discontinued for some time. There has never been an ASME SA-69. One assumes you mean ASME SA-105 "low carbon steel forging material"?? Upvote 0 Downvote
ASTM A-69 has been discontinued for some time. There has never been an ASME SA-69. One assumes you mean ASME SA-105 "low carbon steel forging material"??