Feb 2, 2012 #1 dmkd1 Mechanical Joined Jan 5, 2012 Messages 6 Location IE I am looking to design a vessel with S275 JR steel which is covered by EN 10025-2:2004. However this grade steel is not an option on the Finglow software. Do I use the closest matching material in this case?
I am looking to design a vessel with S275 JR steel which is covered by EN 10025-2:2004. However this grade steel is not an option on the Finglow software. Do I use the closest matching material in this case?
Feb 3, 2012 #2 SJones Petroleum Joined Apr 22, 2001 Messages 3,945 Location GB Is it because S275 is a structural steel? Steve Jones Materials & Corrosion Engineer http://www.linkedin.com/pub/8/83b/b04 Upvote 0 Downvote
Is it because S275 is a structural steel? Steve Jones Materials & Corrosion Engineer http://www.linkedin.com/pub/8/83b/b04
Feb 20, 2012 #3 aburafdi Materials Joined Feb 13, 2012 Messages 48 Location ID Steve is correct! S275JR is not for pressure equipment. Try P265GH, or if you need higher strength : P295GH. Upvote 0 Downvote
Steve is correct! S275JR is not for pressure equipment. Try P265GH, or if you need higher strength : P295GH.
Feb 21, 2012 Thread starter #4 dmkd1 Mechanical Joined Jan 5, 2012 Messages 6 Location IE Thanks! Upvote 0 Downvote