Hi,
I need to procure either S163 or DTD5192. it has been a long hard struggle and I have come up with nothing.
so I was wondering if there is a base material I can procure and heat treat in some way to bring it up to either S163 or DTD5192?
any help would be greatly appreciated.
Thanks
Matbuyer
I need to procure either S163 or DTD5192. it has been a long hard struggle and I have come up with nothing.
so I was wondering if there is a base material I can procure and heat treat in some way to bring it up to either S163 or DTD5192?
any help would be greatly appreciated.
Thanks
Matbuyer