What is the best source for information on stainless steels immersed in warm Chlorine or Bromine water?
 
wahnerma

As a general rule, stainless steels and chlorine are not a good combination. Therefore, a bit more information about your application is necessary. I'm not sure whether you're just looking for some general information about stress corrosion cracking, whether you're looking for material properties for various grades of steel, or whether what you really want is to know the best material to use when you've a process that requires submergence in a warm chlorine or bromine bath (and what is "warm"?)

Patricia Lougheed

Please see FAQ731-376: Eng-Tips.com Forum Policies for tips on how to make the best use of the Eng-Tips Forums.
 
Scenario: submerged machine parts in a hydro-therapeutic environment.
 
Chlorinated/brominated water is very different than bromine- or chlorine-SATURATED water...quite a few orders of magnitude in both bromine/chlorine and bromide/chloride ion concentrations in these two cases.

 