S.S. compatiblity with METHANOL

Status
Not open for further replies.

efm

Mechanical
May 5, 2002
6
I need to know which grade of stainless steel is compatible with METHANOL and what are the reasons .
 
Replies continue below

Recommended for you

mcguire already answered this question in his reply to your previous message (thread330-24939). All stainless steel grades are resistant to methanol, based on the stability of the oxide layer in the presence of an alchohol (methanol is methyl alcohol).
 