I am trying to locate any S-N curve data for BS970 817M40T or equivelant, I believe AISI 4340 is nearly identical. The requested data is to enable some preliminary fatigue calculations to be done, prior to aquiring proper S-N data for a worst case material condition.

Below is typical material mechanical test data for five components.

Please note material diameter is 480mm or 19" which puts it outside the normal ruling section

1 2 3 4 5
------------------------------------------------------
Tensile N/mm2 945 937 954 922 904
Yield N/mm2 757 724 766 724 702
Elongation % 16 16 17 17 16
Reduction of Area % 64 41 48 47 42
Charpy @ 20 C Joules 44 55 49 51 64
Charpy @ 0 Deg C Joules n/a 33 33 39 40

Any data or comments would be appreciated

 
There is a lot of data on 4340 in "Atlas of Fatigue Curves" Edited by H.E.Boyer and available from ASM
 