rust protectant for steel electric motor housings

Status
Not open for further replies.

plouka

Mechanical
Joined
May 30, 2003
Messages
1
Location
US
We are in need of a rust preventative for our steel engines. The coating must dry in about 10 minutes and the coating must last for about a year. Sometimes our motors sit on the shelves (indoors) for about 6 months. If anyone has any information on a product that may meet our specs let me know. Thanks in advance for your help.
 
I would suggest a Vapor phase protection e.g. CORTEC Co
(800)4-CORTEC MN 55110 USA
 