we have seen a lot of rejection for "in line" rusting during our vibro finish processes. This especially becomes the case when there is a short power failure and the parts in the vibrators become extremely prone to rust...we do have power backup but we do see a lot of rejects ...any expert on vibro finishing with recommendations...our process is very suspect and i would be willing to doubt every process paramater.