What is the relationship between shear strength and tensile strength in rubber materials?
 
Replies continue below

Recommended for you

Rubbers [elastomers] have tests similar to metals... but their individual tensile/shear @strain-deformation are highly dependent on their chemistry/cure/form/reinforcing fibers, etc.

NOTHING simple/linear about this answer... which is why no-one has replied.

Regards, Wil Taylor
o Trust - But Verify!
o For those who believe, no proof is required; for those who cannot believe, no proof is possible. [variation, Stuart Chase]
o Unfortunately, in science what You 'believe' is irrelevant. ["Orion", HBA forum]
o Only fools and charlatans know everything and understand everything." -Anton Chekhov
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor