Jul 29, 2020 #1 Mating Materials Joined Jul 29, 2020 Messages 2 Location FR Hi all I need help for a rubber recipe to resist anhydrous ammonia and to have low permeability. I choose to use one of these three rubber : EPDM, IIR and CR. Any Help for the rest of the recipe ? Filler, accelerators, plasticizer ... Thank you
Hi all I need help for a rubber recipe to resist anhydrous ammonia and to have low permeability. I choose to use one of these three rubber : EPDM, IIR and CR. Any Help for the rest of the recipe ? Filler, accelerators, plasticizer ... Thank you
Jul 29, 2020 1 #2 Pete51 Chemical Joined Jul 18, 2013 Messages 6 Location US A peroxide cured EPDM would be an excellent choice. Pete Upvote 0 Downvote
Jul 31, 2020 Thread starter #3 Mating Materials Joined Jul 29, 2020 Messages 2 Location FR Thanks Pete51 for your help. is it better to use filler like CB or clay ? you advise me to use a plasticizer or not? Thanks Upvote 0 Downvote
Thanks Pete51 for your help. is it better to use filler like CB or clay ? you advise me to use a plasticizer or not? Thanks
Aug 5, 2020 #4 Fenty99 Industrial Joined Aug 5, 2020 Messages 5 Location GB Like Pete on this one. Peroxide Cure EPDM rubber. A plasticizer will make the recipe more flexible, not necessarily making it low permeable. Upvote 0 Downvote
Like Pete on this one. Peroxide Cure EPDM rubber. A plasticizer will make the recipe more flexible, not necessarily making it low permeable.