hello can you write me a recipe for rubber tap hose Please
Phr

Rubber. 55

Çinko oksit. 5

Steerik asit 1

Fef N 550. 12

As.....
Please
 
What fluid (and at what temperature) is the hose to carry?

forumtowers.com
 
FB_IMG_1560710511711_qhudgn.jpg
 
For this rubber hose, I need to recycle the dough recipes.
 
Radiator hose usually demands two distinct formulations: 1 for the inside and 1 for the cover because of the fluid being carried in it. EPDM might not necessarily be the correct polymer for the inside. What fluid is to be carried?

forumtowers.com
 
Graham brother can give both formulas respects
 
Terikanli - you still haven't told us which fluid is to be transported in the hose.

forumtowers.com
 
1.Antirriz water 2. Engine oil the 3.benz 4.Dizel
 
Antirriz? = antifreeze?
benz? = petrol/gasoline?

forumtowers.com
 