Rubber desiccant? 1

Status
Not open for further replies.

tom1953

Chemical
Joined
Jul 25, 2005
Messages
177
Location
US
I know calcium oxide is very commonly used as a desiccant in rubber compounds, but I can't use CaO. Are there other desiccants that can be used?

Thanks,
tom
 
It adversely affects the curing of millable polyurethanes.
 
Have you checked with your supplier? They might be able to suggest an alternative.
 
Have you tried MgO? Sometimes it can be used as desiccant because of his hygroscopic nature.
 