Dec 17, 2013 #1 m1208 Structural Joined Apr 6, 2011 Messages 71 Location US What is the weight of 1x4 roof skip sheathing spaced at 7" o.c.?
Dec 17, 2013 2 #2 hokie66 Structural Joined Jul 19, 2006 Messages 23,523 Location AU 1 x 4 made of what material? And don't just say 'wood', as there is a large range of density in wooden products. Honestly...any 6th grade kid should be able to answer your question. Upvote 0 Downvote
1 x 4 made of what material? And don't just say 'wood', as there is a large range of density in wooden products. Honestly...any 6th grade kid should be able to answer your question.
Dec 17, 2013 Thread starter #3 m1208 Structural Joined Apr 6, 2011 Messages 71 Location US IT IS REDWOOD FROM EARLY 1900'S. Upvote 0 Downvote
Dec 18, 2013 #4 TomDOT Materials Joined Sep 15, 2011 Messages 664 Location US Engineering Toolbox gives me a density of 28 lbs/ft3 for American Redwood, 32 for European. Upvote 0 Downvote
Dec 18, 2013 #5 msquared48 Structural Joined Aug 7, 2007 Messages 14,745 Location US So, with that, what are the actual dimensions of a 1X4? Mike McCann MMC Engineering Upvote 0 Downvote
Dec 18, 2013 #6 TomDOT Materials Joined Sep 15, 2011 Messages 664 Location US ...from the early 1900's. Is it rough, or planed? Upvote 0 Downvote
Dec 18, 2013 1 #7 msquared48 Structural Joined Aug 7, 2007 Messages 14,745 Location US If the same planks were used for the Spruce Goose, then they were planed. Mike McCann MMC Engineering Upvote 0 Downvote
If the same planks were used for the Spruce Goose, then they were planed. Mike McCann MMC Engineering
Dec 18, 2013 #8 TomDOT Materials Joined Sep 15, 2011 Messages 664 Location US ....and mostly birch, neither redwood nor spruce. Upvote 0 Downvote