As per SA-480,
"8.1 A report of the results of all tests required by the product
specification shall be supplied to the purchaser".

My concern is: "results" of test shall be in the form of numerical values (for example: Tensile Strength, 460 MPa) OR stated in the notes (remarks) that the properties comply with material specification (see photo-shot below)?
Can smb, pls, help to understand SA-480 requirements.
 

Attachments

  • photo_2025-07-04_12-04-59.jpg
    photo_2025-07-04_12-04-59.jpg
    36.7 KB · Views: 14
If it is a test that is pass/fail then that is OK.
Otherwise I expect numbers.
And 'capable' is never acceptable.
Of course considering the source they are likely to just give you values from some tests that may not be for the lot of material in question at all.
 
If it is a test that is pass/fail then that is OK.
Otherwise I expect numbers.
And 'capable' is never acceptable.
Of course considering the source they are likely to just give you values from some tests that may not be for the lot of material in question at all.

In Certificate in Remarks its says: "1. we hereby certify that the material described herein has been manufactured and tested with satisfactory results in accordance with the requirements of the above material specification". At the same time, herein certificate any values stated for mechanical properties (see screen-shot).

What you mean by "capable"?...where that word comes from?

Pls, help to understand, what ASME Code means by word "results" ? What is definition of "result" as per ASME Code (it means "values" or state "satisfactory", "acceptable"?).
 

Attachments

  • photo_2025-07-05_15-09-40.jpg
    photo_2025-07-05_15-09-40.jpg
    19.7 KB · Views: 6
Seems like you don't trust your metal supplier.

There's no amount of paper that can fix that.
 
I have seen cases where there is a test (maybe a bend test) that always passes and they simply don't want to do it each time.
So they say that it is 'capable' of passing.
In the case of ASME I have always taken results to mean just that.
If it is a measurement I want the numbers, if it is a pass/fail test then tell me how many you did that passed.
This is a procurement problem.
They didn't get what you need.
Let purchasing pay to have the material all retested by an accredited lab.
 