Dear all

what is the resin specifications that I should take care of for crude oil tank bottom plate, we want apply it over fiberglass linning

thank you
 


I looked to my old documents . One of the followings polyesters ( Bisphenol epoxy resin, Vinyl ester resin and polyester resin ) specified.

 