Hi All,

Regarding our specification, production test shall be done for sour service and when the basic code requires it.but our vendor insist to follow his comments:
1-preparing production test piece for each item instead of preparing for every vessel(it means for some vessels with same condition, material,wps only one test piece will be prepared)
2-the hardness test and impact test only are performed for production test, exception of tensile, bending, micro, and macro test.if the hardness&impact test are failed, the omitted test will be done.

please let me know your comments about this matter

Thanks a lot in advance
 
wps is not needed for every vessel of the same.
for sour service, impact/hardness is imperative, so their aproach is good,
if the hardness fail you have to provide more testing to assure the materials comply,
genb
 