Please see the attached sketch. This is for a concrete renovation job where some concrete is spalling due to rebar corrosion. We have a few spots where the hooked end of a horizontal rebar has corroded and need to be replaced. The question is how do we make replace this bar. My solution is to drill next to the horizontal portion of this bar, and install a hooked dowel with Hilti HIT adhesive. This would decrease the depth of the required lap of the new and existing horizontal lengths. Does this sound like a reasonable solution? Any input would be greatly appreciated. Thanks,