Inspector_1998
Mechanical
Hello ,
I have process piping is high critical due to stream fluid ,constructed material is carbon steel ,maximum operation pressure 20 bar and temperature 30C.
piping class 3103 , size 6'' Sch.80 NT=10.97mm . as per the thickness measurement the minim actual thickness 6.0mm and the next opportunity for replacement after three years corrosion rate 0.9mm/year.this is unform corrosion along pipe (sulfidation).
Now, i want to understand when the replacement of process piping constructed as per ASME31.3 REQUIRE , Is there any critical or philosophy behind it ?
when i reviewed the history of process piping in area where i worked , i could not figure out the rule of thumb of replacement .
some piping replaced for the same reason when the corrosion allowance consumed and others not.
API570 and API574 are not covering this point.
regards,
I have process piping is high critical due to stream fluid ,constructed material is carbon steel ,maximum operation pressure 20 bar and temperature 30C.
piping class 3103 , size 6'' Sch.80 NT=10.97mm . as per the thickness measurement the minim actual thickness 6.0mm and the next opportunity for replacement after three years corrosion rate 0.9mm/year.this is unform corrosion along pipe (sulfidation).
Now, i want to understand when the replacement of process piping constructed as per ASME31.3 REQUIRE , Is there any critical or philosophy behind it ?
when i reviewed the history of process piping in area where i worked , i could not figure out the rule of thumb of replacement .
some piping replaced for the same reason when the corrosion allowance consumed and others not.
API570 and API574 are not covering this point.
regards,